Robotic MAG Fillet Welding Procedure Specification for S235JR Steel Plates

0.0(0 reviews)
Robotics
Robotic Mag Welding
Fillet Welding
S235Jr Steel
Welding Procedure Specification
Logo
sprite x=0 y=0
Angle x=0 y=0
Angle x=0 y=90
Angle x=0 y=270
Angle x=90 y=0
Angle x=270 y=0
Angle x=60 y=30

About this design

Comprehensive guide on preparing a preliminary Welding Procedure Specification (pWPS) for robotic MAG fillet welding on 8 mm S235JR steel plates. Includes thermal and mechanical simulation analysis to optimize welding parameters, shielding gas, and filler wire selection in compliance with EN ISO standards.

What people convert this model to

Loading conversion stats…

Download this model

Pick the format your software opens. The native file is free.

Opens in SolidWorks, Fusion, Onshape, Inventor. Need a mesh or a drawing? Pick a format above.

<100
<100

The files are shared to help you get inspired and speed up your workflow. They may not be fully accurate or production-ready, so review carefully before use.

View NameExtensionAction
Design fileFormat: STEP
Front Viewwebp
Top Viewwebp
Bottom Viewwebp
Left Side Viewwebp
Right Side Viewwebp
Isometric Viewwebp
Supporting Files (0)
PreviewFile NameAction
No supporting files

CAD File Details

File Information
File Name69806ba0623f1239fccaacb0_...
File TypeSTEP
Unitsmm
Geometry Summary
Faces10
Edges24
Vertices16
Solids1
Surface Types
Planar10
Cylindrical0
Conical0
Spherical0
Toroidal0
Other0
Bounding Box
Width200.00 mm
Height150.00 mm
Depth158.00 mm
Volume
Max Volume480000.00 mm³
Min Volume480000.00 mm³
Average Volume480000.00 mm³
Total Volume480000.00 mm³
Usage Notes
NotesSuitable for design reference, visualization, prototyping workflows and engineering review. Validate dimensions and geometry before manufacturing use.

What you can use this CAD model for

  • Engineering review
  • Manufacturing discussion
  • Supplier communication
  • Prototype development
  • Design validation

Before using this CAD file

Review the model dimensions, units and geometry before using it for manufacturing or production. Some files may be created for reference, visualization or workflow acceleration and may require validation before final use.

Paid Pipeline · $5.99 per drawing set

Need 2D engineering drawings for this CAD model?

Generate multi-view 2D technical drawings from this 3D CAD file, including orthographic views, section cuts and downloadable PDF, SVG and DXF files.

  • ✓ Usually ready in minutes
  • ✓ 9 sheets · editable FCStd + PDF, SVG, DXF
  • ✓ No subscription · pay per file
$5.99
per drawing set incl. GST
4 min
avg. turnaround

Comments

0
Y
Loading comments...

Marathon-OS Design Hub

Everything you need to design faster, smarter, and with more impact.

3D Printed Vase 4 | Industrial CAD Design
3D Printed Vase 4 | Industrial CAD Design
Parabiaugmented Truncated Dodecahedron | 3D Engineering Design File
Parabiaugmented Truncated Dodecahedron | 3D Engineering Design File
Prateleira De Livro Em Homenagem Ao Ayrton Senna Sennasempre 1 | 3D CAD Engineering Model
Prateleira De Livro Em Homenagem Ao Ayrton Senna Sennasempre 1 | 3D CAD Engineering Model
Multi-Drum Machine Mounting Plate Design
Multi-Drum Machine Mounting Plate Design
69 Pulley Gt2 3D Print Cnc Fusion 360 Pistacchio Graphic | 3D CAD Engineering Model
69 Pulley Gt2 3D Print Cnc Fusion 360 Pistacchio Graphic | 3D CAD Engineering Model
Diy 3D Photobooth 1 | 3D CAD Engineering Model
Diy 3D Photobooth 1 | 3D CAD Engineering Model
Bass Sign 2 | 3D CAD Engineering Model
Bass Sign 2 | 3D CAD Engineering Model
GoPro Hero 11 Mini
GoPro Hero 11 Mini
3D Printer Core Xy Diy - Standard Mechanical Component
3D Printer Core Xy Diy - Standard Mechanical Component
Box With Hinges For 3D Printing | 3D Engineering Design File
Box With Hinges For 3D Printing | 3D Engineering Design File
Ice Cube Tray | 3D Engineering Design File
Ice Cube Tray | 3D Engineering Design File
3D Model of a Chess King Piece - CAD Design Tutorial
3D Model of a Chess King Piece - CAD Design Tutorial
3D Printed Protective Case for Environmental Sensor
3D Printed Protective Case for Environmental Sensor
E3D Revo | High-Quality CAD Model
E3D Revo | High-Quality CAD Model
Ducto Optimizado Ender 3 Parta Barrel Bimetal 1 | 3D CAD Engineering Model
Ducto Optimizado Ender 3 Parta Barrel Bimetal 1 | 3D CAD Engineering Model
Buoyant Ball 1 | 3D CAD Engineering Model
Buoyant Ball 1 | 3D CAD Engineering Model
View all designs

Recently added / Trending

Everything you need to design faster, smarter, and with more impact.

Corner For Hygenic Air Handling Unit - Downloadable CAD Representation
Corner For Hygenic Air Handling Unit - Downloadable CAD Representation
UAV Aircraft Model for Engineering and Design
UAV Aircraft Model for Engineering and Design
Bismarck 1 | 3D CAD Engineering Model
Bismarck 1 | 3D CAD Engineering Model
Oil Fired Boiler Vertical Boiler Steam Locomotive Boiler 1 | 3D CAD Engineering Model
Oil Fired Boiler Vertical Boiler Steam Locomotive Boiler 1 | 3D CAD Engineering Model
Panel Switch Power
Panel Switch Power
Blow Mold Bottle Sergio Cam
Blow Mold Bottle Sergio Cam
Main Distribution Switchboard - Downloadable CAD Representation
Main Distribution Switchboard - Downloadable CAD Representation
CAD Model of Fuse Holder for Engineering Projects
CAD Model of Fuse Holder for Engineering Projects
Female Obd2 Connector With Straight Pins - Downloadable CAD Representation
Female Obd2 Connector With Straight Pins - Downloadable CAD Representation
Musgres V2 | 3D Engineering Design File
Musgres V2 | 3D Engineering Design File
View all designs

Free Online CAD Viewer –Secure, Fast & Cloud-Based

A lightweight, online tool to convert 3D file formats—anytime, anywhere, without installing any software.

Drag & drop your 3D files

Supported formats: STEP (.step, .stp), IGES (.igs, .iges), STL (.stl), PLY (.ply), OFF (.off), BREP (.brp, .brep)

upload
Don't have a file? Try one of these samples:


CAD Viewer featureOpen CAD files instantly in your browser.
CAD Viewer featureNo software needed.
CAD Viewer featurePrivate uploads.
CAD Viewer featureAutomatically deleted after 7 days.
CAD Viewer featureUpload files up to 300 MB